Hey all. I've recently started a mask project and wanted to start with a full headcast first. Pretty standard two part mold affair. Unfortunately i completely goofed and bought the wrong silicone. I got a slow platinum silicone with a cure time of 3-4 hours. Don't get me wrong, the test strip on the back of my hand turned out to be amazing in quality, but not really workable for a headcast.
My question is, would adding a thickening agent and an accelerator be worth it, or should i just accept my losses and get the correct high viscosity, fast working silicone instead?